LOCTITE ABLESTIK DX20C

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK DX20C

Main features

  • Translucent
  • Non conductive
  • For GaN LEDs

Product Description

LOCTITE ABLESTIK DX20C dielectric adhesive offers excellent adhesion strength, especially at wire bonding process temperature to minimize defect rate at assembly. It features strong heat / UV resistance and can be applied by pin transfer, stamping and dispensing.

LOCTITE ABLESTIK DX20C is a translucent, one component die attach that doesn't yellow and has excellent adhesion for LED applications on GaN (Gallium Nitride) substrates.

 

Cure Schedule

  • 1 hour @ 170°C
Product Family

ABLESTIK DX20C

No longer available

This product is no longer available from Krayden. Please contact us so we can recommend an alternative product.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.17
Work life @25°CWork life @25°C
120 hours
Chemical Properties
Moisture absorptionMoisture absorption
0.6 %
Physical Properties
ViscosityViscosity
12,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers