ABLESTIK 369-3
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

Main features
- 0.0005 ohm-cm Volume Resistivity
- 4-Hour 74 deg C Cure
- Two-Hour Working Window
Product Description
LOCTITE® ABLESTIK 369-3 is a silver-filled, electrically conductive epoxy adhesive for die-attach and general-purpose bonding applications. The polyamine-activated system provides a two-hour work life at 25°C and uses a moderate-temperature guideline cure of 4 hours at 74°C. Typical cured properties include volume resistivity of 0.0005 ohm-cm, Shore D hardness of 80, and aluminum-to-aluminum lap shear strength of 7.6 N/mm² at 25°C.
Key features
- Electrically conductive: Typical cured volume resistivity is 0.0005 ohm-cm.
- Moderate-temperature cure: Guideline cure schedule of 4 hours at 74°C.
- Extended processing window: A two-hour work life at 25°C supports adhesive placement before cure.
Applications / Suitable for
- Die-attach applications
- General-purpose conductive bonding
- Aluminum-to-aluminum bonding under the documented test condition
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical component, work-life, storage, and guideline cure information before final processing.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Technology | Epoxy | — | Polyamine-activated adhesive system |
| Appearance | Silver paste | — | Both Part A and Part B |
| Filler type | Silver | — | Conductive filler |
| Specific gravity — Part A | 3.0 | — | SDS physical-property value |
| Specific gravity — Part B | 3.4 | — | SDS physical-property value |
| Work life | 2 | hours | At 25°C |
| Guideline cure schedule | 4 | hours | At 74°C |
| Optimal storage — Part A | -40 | °C | Store at or below -40°C; unopened container |
| Optimal storage — finished adhesive | -40 | °C | TDS storage recommendation |
After-processing / final-state properties
Typical cured-material electrical, physical, and bonded-joint properties. Values are reference data and are not product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 80 | Shore D | Cure condition and test method not stated |
| Volume resistivity | 0.0005 | ohm-cm | Test method, specimen geometry, and cure condition not stated |
| Lap shear strength — aluminum to aluminum | 7.6 (1,100) | N/mm² (psi) | Tested at 25°C; surface preparation, bondline, cure condition, and test method not stated |