LOCTITE ABLESTIK 2100A

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 2100A

Main features

  • Fast cure
  • High hot/wet adhesion
  • Ultra low moisture absorption

Product Description

LOCTITE ABLESTIK 2100A die attach adhesive is designed for Pb-free array packaging. This product is able to withstand the high reflow temperatures necessary for Pb-free solders @260°C. It is the "Go To" product for conductive laminate.

LOCTITE ABLESTIK 2100A is a low stress, low bleed conductive die attach with ultra low moisture absorption, suitable for laminate packages like BGA and die sizes up to 12.7 x 12.7 mm

Cure Schedule

  • 30 minute ramp to 175°C + 15 minutes @ 175°C

 

Product Family

ABLESTIK 2100A

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
60 °C
Thermal ConductivityThermal Conductivity
1.2 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
0.05 Ohms⋅cm
Physical Properties
Thixotropic indexThixotropic index
5.3
ViscosityViscosity
9,000 mPa.s

Additional Information

ABP 2100A is containing a PFAS anti-bleed agent and will be discontinued as Henkel moves towards greener materials. The direct PFAS-free replacement is ABP 2100ANP, with only minor changes. Notification is planned for January 2026, with the last-time-buy in December 2026.

Loctite Ablestik 2100A is a product that is an almost direct alternative to Loctite Ablestik 2000B.

Loctite Ablestik 2000B is also a conductive die attach for laminates that it is mainly used in Asian regions. For EMEA we have successfully used 2100A as a drop in for use in BGA laminate applications with great success rates.



Ablestik 2100A DSC Curve - Heat flow vs temperature



Notice how the Onset of cure (minimum cure temperature) is about 70°C. Even though we suggest curing at 175°C, as with all products you can adjust the cure schedule (with a lot of trial, error and personal work) according to your final application properties. 

The volume resistivity may be reduced when curing below 175°C (compared to the TDS value), but we expect that some conductivity will be developed.

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers