Main features
- Structural Bonding And Fairing
- Selectable Assembly Work Life
- Sandable Non Sag Gap Filling
Product Description
3M Scotch-Weld Structural Adhesive EC-3587 B/A Gray is a gray, two-part polyurethane structural adhesive available in B-1/4 and B-1 work-life classes. It cures at room temperature or with heat to a tough, impact-resistant material that bonds many prepared metal and plastic substrates. The non-sag mixture also functions as a void filler or fairing compound and can be sanded after cure. Class B-1/4 provides 5 to 20 minutes of work life, while Class B-1 provides 40 to 150 minutes at 23 deg C for different part sizes and placement windows.
Key features
- Structural Bonding And Fairing: One material can bond, fill gaps, and form a sandable fairing surface.
- Selectable Work Life Classes: B-1/4 and B-1 versions provide different application windows.
- Tough Non Sag Urethane: The mixed adhesive holds its shape and cures to an impact-resistant material.
Applications
Structural bonding of prepared metals and plastics, void filling, gap filling, and sandable fairing work.
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
Processing values are separated by B-1/4 and B-1 class where they differ.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Available classes | B-1/4; B-1 | - | Select before processing |
| Solids | 100 | % | Both components and both classes |
| Mix ratio by weight | 100:100 | B:A | Both classes |
| Mix ratio by volume | 175:100 | B:A | Both classes |
| B-1/4 work life | 5 to 20 | min | 100 g mixed at 23 deg C |
| B-1 work life | 40 to 150 | min | 100 g mixed at 23 deg C |
| Mixed flow | 0.1 | in | MIL-S-8802 Figure 1 |
After-processing / final-state properties
Cured overlap-shear results remain separated by B-1/4 and B-1 class.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 62 | Shore D | Cured; both classes |
| B-1/4 overlap shear | 3390 | psi | FPL-etched aluminum; tested at -40 deg C |
| B-1 overlap shear | 3765 | psi | FPL-etched aluminum; tested at -40 deg C |
| B-1/4 overlap shear | 2450 | psi | FPL-etched aluminum; tested at 24 deg C |
| B-1 overlap shear | 2512 | psi | FPL-etched aluminum; tested at 24 deg C |
| B-1/4 overlap shear | 476 | psi | FPL-etched aluminum; tested at 82 deg C |
| B-1 overlap shear | 475 | psi | FPL-etched aluminum; tested at 82 deg C |