3M EC-3501

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3501

Main features

  • Rapid Structural Repair Bonding
  • Controlled Composite Defect Filling
  • High Room Temperature Shear

Product Description

3M Scotch-Weld Epoxy Adhesive EC-3501 B/A Gray is a gray, rapid-curing two-part epoxy for structural bonding and surface repair on prepared metals, composites, and selected plastics. Equal-volume mixing, a 6 to 10 minute work life at 24 deg C, and thixotropic flow support controlled placement in short-cycle assembly or repair. It can fill pinholes and localized surface porosity in cured fiber composites. After cure, the adhesive reaches Shore D 75 to 80 hardness and delivers 3200 psi aluminum overlap shear at 24 deg C with FPL-etched adherends.

Key features

  • Rapid Room Temperature Cure: A 6 to 10 minute work life supports short-cycle bonding and repair.
  • Composite Surface Repair: The epoxy fills localized porosity and pinholes in cured fiber composites.
  • Controlled Thixotropic Flow: High viscosity limits migration after the mixed adhesive is placed.

Applications

Structural bonding of prepared metals, composites, and selected plastics; localized porosity and pinhole repair in cured fiber composites.

Product Family

3M EC-3501

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity (Part A)Viscosity (Part A)
20-35 mPa.s
Viscosity (Part B)Viscosity (Part B)
40-55 mPa.s
General Properties
ColorColor
Gray
Mix RatioMix Ratio
1:1
Electrical Properties
Dielectric StrengthDielectric Strength
27.56 kV/mm
Volume ResistivityVolume Resistivity
1.2 x 10 ^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorWhite-Base before mixing
Part A colorBlack-Accelerator before mixing
Mix ratio by volume1:1B:ATwo-part system
Mix ratio by weight1.05:1B:ATwo-part system
Base press-flow time15 to 40secAt 24 deg C
Accelerator press-flow time35 to 60secAt 24 deg C
Work life6 to 10min20 g mixed at 24 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorGray-Cured
Hardness75 to 80Shore DCured
Overlap shear strength1500psiFPL-etched aluminum; tested at -55 deg C
Overlap shear strength3200psiFPL-etched aluminum; tested at 24 deg C
Overlap shear strength500psiFPL-etched aluminum; tested at 82 deg C
T-peel strength4piwAluminum; tested at 24 deg C
Dielectric strength700V/milCured adhesive

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers