3M 950
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- 5 mil Adhesive 300 Construction
- High Initial Adhesion and Holding
- Multi-Substrate Pressure-Sensitive Bonding
Product Description
3M™ Adhesive Transfer Tape 950 is a 5 mil (0.13 mm) adhesive transfer tape featuring 3M™ Adhesive 300, a pressure-sensitive, medium-firm, fibered acrylic adhesive supplied on a tan 60# glassine liner. It provides very high initial adhesion with good holding power across a range of materials, including metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.
Key features
- High initial adhesion: 3M™ Adhesive 300 provides strong initial bonding with good holding power.
- Broad substrate compatibility: Bonds to metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.
- Conformable 5 mil adhesive: The 0.13 mm adhesive thickness supports bonding to surfaces where texture may be visible.
- Environmental resistance: Provides resistance to humidity, water, UV exposure, temperature cycling, oil, mild acids, and mild alkalis when properly applied.
- UL-recognized construction: Recognized under UL 969 for Marking and Labeling Systems Materials Components.
Applications / Suitable for
- Bonding graphic nameplates and overlays
- Attaching metal nameplates and rating plates
- Laminating foam for gasket applications
- Joining similar and dissimilar industrial materials
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Adhesive Layer
300 Fibered Acrylic A layer that is applied to one surface or both to bind items together and resist their separation
Release Liner
Tan 60# Glassine A paper or plastic-based film sheet used to prevent a sticky surface from prematurely adhering
Total Thickness
130 μm Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
Additional Information
Technical properties
As-supplied / before-processing properties
Representative or typical product properties. Values should not be used for specification purposes.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive type | 3M™ Adhesive 300, fibered acrylic | — | Pressure-sensitive, medium-firm acrylic |
| Total tape thickness | 0.13 (5) | mm (mil) | ASTM D3652 |
| Liner | 60# glassine | — | Tan primary liner |
| Liner thickness | 0.08 (3.2) | mm (mil) | Published typical value |
| 90° peel adhesion — ABS | 3.7 (34); 4.4 (40) | N/cm (oz/in) | ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| 90° peel adhesion — polypropylene | 6.6 (60); 6.8 (62) | N/cm (oz/in) | ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| 90° peel adhesion — stainless steel | 8.1 (74); 9.4 (86) | N/cm (oz/in) | ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| Short-term temperature resistance | 121 (250) | °C (°F) | Short term: minutes or hours |
| Long-term temperature resistance | 70 (158) | °C (°F) | Long term: days or weeks |
| Lower temperature service limit | -40 (-40) | °C (°F) | Properly applied tape |
| Coefficient of thermal expansion — first heat | 20 × 10-5 | m/m/°C | ASTM D696 |
| Coefficient of thermal expansion — second heat | 58 × 10-5 | m/m/°C | ASTM D696 |
| Dielectric constant | 3.21 | — | ASTM D150; 23°C (73°F); 1 kHz |
| Dissipation factor | 0.04 | — | 23°C (73°F); 1 kHz |
| Dielectric strength | 340 | V/mil | ASTM D149; 500 VAC RMS, 60 Hz/sec |
| Shelf life | 24 | months | From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging and out of direct sunlight |