3M™ Double-Sided Paper Tape 9086
Harmonization Code : 4811419000 | Self-adhesive paper paperboard printed rolls sheets
Main features
- Bonds to a wide variety of substrates
- 0.5 mil tissue carrier
- Double coated with 3.5 mil adhesive on each side
Product Description
3M™ High Performance Double Coated Tape 9086 is a double-sided tape featuring a conformable tissue carrier coated with 3M™ 375 acrylic adhesive on both sides. Designed for high-performance bonding, it delivers very high initial tack along with excellent peel and shear strength across a wide range of substrates, including textured and difficult-to-bond surfaces. The 0.5 mil tissue carrier allows for easy hand tearing and conformability, while the glassine liner ensures smooth and efficient application.
Product Key Features
- 3M™ 375 adhesive provides very high initial tack with excellent peel and shear strength
- 3.5 mil adhesive on each side ensures strong bonding on multiple surfaces
- Bonds to metals, glass, foams, painted surfaces, and various plastics, including difficult-to-stick materials
- 0.5 mil carrier adapts well to irregular and textured surfaces
- Suitable for use in hand dispensers for controlled placement
Applications
- Zero-speed and general splicing operations
- Point-of-purchase (POP) and display assembly
- Fabric bonding and textile applications
- Blind manufacturing and assembly
- Print finishing and graphic mounting
- General-purpose bonding of smooth, rough, or textured materials
Packaging
Please select Width, Length, Thickness and Color.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Color
Translucent The color
Total Thickness
19 μm Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.