3M 604NS
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Non-Sag Vertical Gap Filling
- Rapid 4-Minute Working Window
- Multi-Material Structural Bonding
Product Description
3M Scotch-Weld Urethane Adhesive 604NS is a two-part, non-sag polyurethane adhesive for structural and semi-structural bonding where gap filling and vertical or overhead application are important. In the DP604NS Duo-Pak configuration, the 1:1 components dispense as a bubble-free non-sag paste with a typical 4-minute work life, 20-minute tack-free time, and 6-hour full cure at 25 deg C. The adhesive is used with concrete, ceramic, wood, glass, metals, plastics, and rubber in construction, maintenance, and assembly work. Its rapid setting profile and sag resistance suit bonded joints that must stay in place during cure.
Key features
- Non-sag gap filling: The mixed adhesive stays as a non-sag paste for vertical and overhead bonding while filling joint gaps.
- Rapid working and cure: DP604NS has a typical 4-minute work life, 20-minute tack-free time, and 6-hour full cure at 25 deg C.
- Multi-material structural bonding: The adhesive is used with concrete, ceramic, wood, glass, metals, plastics, and rubber in construction and assembly work.
Applications
Applications include structural and semi-structural bonding of concrete, ceramic, wood, plastics, rubber, metals, glass, and selected construction assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
DP604NS black Duo-Pak configuration; component data are shown at the stated conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Part A viscosity | 1493 | cP | Typical; HBDVI + CP, 25 deg C |
| Part B viscosity | 1237 | cP | Typical; HBDVI + CP, 25 deg C |
| Mix ratio | 1:1 | DP604NS Duo-Pak components | |
| Shelf life | 6 | months | Unopened package; 18 to 30 deg C |
After-processing / final-state properties
DP604NS black data; final properties apply under the stated cure and test conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 85 | Shore A | Typical; ASTM D2240-91; after full cure |
| Lap shear strength | 900 | psi | Typical; ASTM D1002-72; 7 days at 25 deg C |
| Continuous temperature range | -51 to 121 | deg C | Typical; PEC |