3M 231/231A
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Instant-Adhesion Paint Masking
- Clean Multiple-Bake Removal
- Conformable Mini-Crepe Backing
Product Description
3M Paint Masking Tape 231/231A is a tan, smooth mini-crepe paper tape for industrial and aerospace paint masking, including multiple-bake finishing operations. Its rubber adhesive provides instant adhesion and holding power, while the heat-resistant, solvent- and moisture-resistant backing conforms around complex shapes and tears cleanly for efficient application. Typical construction values include 0.19 mm total thickness, 10% elongation at break, and 49 N/cm tensile strength. The tape provides clean removal following a 30-minute exposure at temperatures up to 149 deg C under the stated condition and is suited to painting automobiles, aircraft, trucks, boats, and fabricated parts. Best results are obtained when it is applied and removed within 24 hours.
Key features
- Instant paint-mask adhesion: The rubber adhesive sticks quickly and resists lifting or curling during supported finishing work.
- Multiple-bake clean removal: The tape removes cleanly after 30 minutes at temperatures up to 149 deg C under the stated condition.
- Conformable mini-crepe backing: The smooth backing follows complex shapes, resists bleed-through, and tears cleanly.
Applications
Applications include industrial paint masking, aerospace masking, multiple-bake finishing, and painting automobiles, aircraft, trucks, boats, and fabricated parts.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Tan | - | Typical |
| Backing | Smooth mini-crepe paper | - | Heat-resistant saturant |
| Adhesive | Rubber | - | Typical |
| Total thickness | 0.19 (7.6) | mm (mil) | ASTM D3652 |
| Elongation at break | 10 | % | ASTM D3759 |
| Tensile strength | 49 (28) | N/cm (lb/in) | ASTM D3759 |
Final-state / after-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180 deg peel adhesion | 4.1 (38) | N/cm (oz/in) | ASTM D3330 at 23 deg C; 304 mm/min |
| Clean-removal bake resistance | Up to 149 (300) | deg C (deg F) | 30 min |
| Recommended indoor exposure | Apply and remove within 24 | h | Best-results condition |
| Backing resistance | Solvent and moisture resistant | - | Applied tape |